Polymer Property : Flexural Modulus = 0.0770 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0770 GPa
11.2 ksi
ASTM D790
DuPont Elvax® 670 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Flexural Modulus 0.0770 GPa
11.2 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Arkema Group Pebax® 4033 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 4033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
Flexural Modulus 0.0770 GPa
11.2 ksi
Conditioned 15 days at 23°C - 50% RH; ISO178
Arkema Group Pebax® 4033 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 4033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
Flexural Modulus 0.0770 GPa
11.2 ksi
ASTM D638
Arkema Group LOTRYL® 14 MGC 02 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 14 MGC 02 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the Methyl Acrylate content, LOTRYL® 14 MGC 02 is a polymer o..
Flexural Modulus 0.0770 GPa
11.2 ksi
Conditioned 15 days at 23°C - 50% RH; ISO178
Arkema Group Pebax® 4033 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 4033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..