Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0650 GPa | 9.43 ksi | ASTM D790 |
C.O.I.M. LARIPUR® LPR107-93A Seal Grade TPU Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |