Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0344 - 0.0482 GPa | 4.99 - 6.99 ksi | Secant 1%; ASTM D-790-95 |
Multibase Multi-Flex® TPO DEFA 1047 The burn rate is 0.53 in/min; ASTM FM VSS 302.Data provided by Multibase. |
|||
Flexural Modulus | 0.0344 GPa | 4.99 ksi | ASTM D790 |
Diamond Polymers Softflex® SF 6060 Thermoplastic Elastomer Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |