Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0180 GPa @Temperature 49.0 °C |
2.61 ksi @Temperature 120 °F |
ASTM D790 |
DuPont Elvax® 450 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Flexural Modulus | 0.0180 GPa | 2.61 ksi | ASTM D638 |
Arkema Group LOTRYL® 24 MA 005 Copolymer Ethylene - Methyl Acrylate LOTRYL® 24 MA 005 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 24 MA 005 is a poly.. |