Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0131 GPa | 1.90 ksi | 1% secant; ASTM D790 |
ExxonMobil Escorene® UL 7710 Adhesive Application Resin Escorene Ultra UL 7710 is a very high flow, 26.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt .. |
|||
Flexural Modulus | 0.0131 GPa | 1.90 ksi | 1% secant; ASTM D790 |
ExxonMobil Escorene® UL 7710E Adhesive Application Resin Escorene Ultra UL 7710E is a very high flow, 26.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt.. |