Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.00900 GPa | 1.31 ksi | 1% Secant |
Advanced Elastomer Systems Vistaflex® 671N Thermoplastic Rubber
(discontinued **) A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 9.0 MPa (1300 psi); Vica.. |
|||
Flexural Modulus | 0.00900 - 0.130 GPa | 1.31 - 18.9 ksi | Average value: 0.0566 GPa Grade Count:17 |
Overview of materials for EMAAA Terpolymer This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Flexural Modulus | 0.00900 GPa | 1.31 ksi | 1% Secant, ASTM D790 |
ExxonMobil Escorene® LD-781 High EVA Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 33% vinyl acetate copolymer for specialty compounding applications. The resin provides excellent stress cracking and flexibility, and allows outs.. |
|||
Flexural Modulus | 0.00900 GPa | 1.31 ksi | ASTM D638 |
Arkema Group LOTRYL® 30 BA 02 Copolymer Ethylene - Butyl Acrylate LOTRYL® 30 BA 02 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 30 BA 02 is used for polymer modification, in compounds formula.. |
|||
Flexural Modulus | 0.00900 GPa | 1.31 ksi | ASTM D638 |
Arkema Group LOTADER® 4603 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4603 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure process in autoclave reactor. LOTADER 4603 is a multipurpose extrusion adhesive used.. |