Mechanical Properties Metric English Comments
Flexural Modulus 0.00630 GPa

@Temperature 23.0 °C
0.914 ksi

@Temperature 73.4 °F
ASTM D790
DuPont Performance Polymers VESPEL TP-8311 Polyimide
Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in both dry and lubricated high temperature environmentsInformation provided b..