Polymer Property : Flexural Modulus = 0.00427 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.00427 - 2.62 GPa
0.620 - 380 ksi
Average value: 0.743 GPa Grade Count:7
Overview of materials for Polycarbonate/Thermoplastic Polyurethane Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Thermoplastic Polyurethane Blend". Each property range of values reported is minimum and m..
Flexural Modulus 0.00427 GPa
0.620 ksi
ASTM D790
Lubrizol Estane® ALR PC73A Thermoplastic Polyurethane
Type: Estane® ALR PC73A is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi..