Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.00300 - 0.190 GPa | 0.435 - 27.6 ksi | 2% Secant; ASTM D790 |
Dow Engage® Polyolefin Elastomer Engage® thermoplastic elastomers are ethylene octene copolymers produced via advanced INSITE™ catalyst and process technology, allowing control over polymer structure, properties, and rheology. .. |