| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Unnotched |
1.27
J/cm <br>@Thickness 3.20 mm,<br> Temperature -30.0 °C
|
2.39
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature -22.0 °F
|
ASTM D256 |
|
LG Chemical LG749W ABS, Low Gloss, Heat Resistance
Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automotive Interior Housing (Glove Cover, Door S/W Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by..
|
|||
| Izod Impact, Unnotched |
1.27
J/cm <br>@Thickness 6.40 mm,<br> Temperature -30.0 °C
|
2.39
ft-lb/in <br>@Thickness 0.252 in,<br> Temperature -22.0 °F
|
ASTM D256 |
|
LG Chemical MP220 ABS, High Adhesion, Heat Resistance
Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical
|
|||
| Izod Impact, Unnotched |
1.27
J/cm <br>@Thickness 3.20 mm,<br> Temperature -30.0 °C
|
2.39
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature -22.0 °F
|
ASTM D256 |
|
LG Chemical MP220 ABS, High Adhesion, Heat Resistance
Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical
|
|||