Polymer Property : Izod Impact, Unnotched = 16.2 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 8.67 J/cm

@Temperature 23.0 °C
16.2 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp PFL34 PA 6
LNP* Lubricomp* PFL34 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am..