Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.981 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
1.84 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Izod Impact, Unnotched | 0.981 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.84 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Izod Impact, Unnotched | >= 0.981 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
>= 1.84 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ISO 180 |
LG Chemical EM500 Impact modifier for Engineering Plastics Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi.. |
|||
Izod Impact, Unnotched | >= 0.981 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
>= 1.84 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ISO 180 |
LG Chemical EM500A Impact modifier for Engineering Plastics Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi.. |
|||
Izod Impact, Unnotched | >= 0.981 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
>= 1.84 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ISO 180 |
LG Chemical EM505 Impact modifier for Engineering Plastics Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi.. |
|||
Izod Impact, Unnotched | 0.981 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
1.84 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ER451 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Izod Impact, Unnotched | 0.981 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
1.84 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Unnotched | 0.981 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.84 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Unnotched | 0.981 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.84 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LG703W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided.. |
|||
Izod Impact, Unnotched | 0.981 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.84 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical XR401B ABS, High Flow, Heat Resistance Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p.. |
|||
Izod Impact, Unnotched | 0.981 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
1.84 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical XR419 ABS, Heat Resistance, Chemical Resistance Feature: Injection Molding, Heat Resistance, Chemical ResistanceApplication: Automotives Interior Housing (Ventgrille Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provide.. |
|||
Izod Impact, Unnotched | 0.981 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.84 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical XR419 ABS, Heat Resistance, Chemical Resistance Feature: Injection Molding, Heat Resistance, Chemical ResistanceApplication: Automotives Interior Housing (Ventgrille Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provide.. |
|||
Izod Impact, Unnotched | 0.981 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
1.84 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ER461 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Izod Impact, Unnotched | 0.981 J/cm @Thickness 6.40 mm, Temperature -20.0 °C |
1.84 ft-lb/in @Thickness 0.252 in, Temperature -4.00 °F |
ASTM D256 |
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical |
|||
Izod Impact, Unnotched | 0.981 J/cm @Thickness 3.20 mm, Temperature -20.0 °C |
1.84 ft-lb/in @Thickness 0.126 in, Temperature -4.00 °F |
ASTM D256 |
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical |
|||
Izod Impact, Unnotched | 0.981 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.84 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical XR401F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Door Frame)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical |