Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.908 J/cm @Thickness 12.7 mm |
1.70 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP310E Cotton Fabric Description: Manufactured with a domestic cotton fabric and phenolic resin. Similar to NP310 with improved moisture resistance and electrical properties. Mechanical properties equivalent to NP310. M.. |
|||
Izod Impact, Unnotched | 0.908 J/cm @Thickness 12.7 mm |
1.70 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP313 Cotton Fabric Description: Canvas phenolic laminate with molybdenum disulfide lubricant. Mechanical properties slightly lower than NP310.Thickness Tested: 0.062", 0.125" & 0.500" |
|||
Izod Impact, Unnotched | 0.908 J/cm @Thickness 12.7 mm |
1.70 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP315 Cotton Fabric Description: Canvas phenolic laminate with graphite added as a solid lubricant. This material has improved wear properties under certain conditions. Material is conductive to electricity and should .. |
|||
Izod Impact, Unnotched | 0.908 J/cm @Thickness 12.7 mm |
1.70 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP320 Cotton Fabric Description: Fine weave (less than 4 ounce/square yard) cotton fabric commonly called linen, combined with phenolic resin to provide better machining than NP310. For smaller and more intricate shape.. |
|||
Izod Impact, Unnotched | 0.908 J/cm @Thickness 12.7 mm |
1.70 ft-lb/in @Thickness 0.500 in |
CW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP342 Cotton Fabric Description: Fine weave canvas phenolic material with fabric construction weight intermediate to NP310 and NP320. Designed for better machining than grade NP310 and lower cost than NP320.Thickness T.. |
|||
Izod Impact, Unnotched | 0.908 J/cm @Thickness 12.7 mm |
1.70 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP344 Cotton Fabric Description: Fine weave canvas laminate with high temperature phenolic resin and molybdenum disulfide lubricant. Good machining properties and low coefficient of thermal expansion. Better machining .. |
|||
Izod Impact, Unnotched | 0.908 J/cm @Thickness 12.7 mm |
1.70 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP424 Laminate Description: Composite material composed of woven glass fabric surfaces and paper core combined with epoxy resin. Primarily used in the printed circuit board industry. Easy punching and excellent el.. |
|||
Izod Impact, Unnotched | 0.910 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.70 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Lubrizol Isoplast® 2531 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Izod Impact, Unnotched | 0.910 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.70 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Lubrizol Isoplast® 301 Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |