Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.883 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
1.65 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LG703W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided.. |
|||
Izod Impact, Unnotched | 0.883 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
1.65 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical XR401B ABS, High Flow, Heat Resistance Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p.. |
|||
Izod Impact, Unnotched | 0.883 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.65 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical XR401 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 .. |
|||
Izod Impact, Unnotched | 0.883 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
1.65 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical XR401F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Door Frame)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical |