Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.490 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical AF342F ABS, Flame Retardant, High Flow Feature: Injection Molding, Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided .. |
|||
Izod Impact, Unnotched | 0.490 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical XR440 ABS, Low Emission High Heat ABS Feature: Injection Molding Grade, Low Emission High Heat ABSApplication: Automotives Interior housingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |
|||
Izod Impact, Unnotched | 0.490 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical XR474F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Exterior Housing (Lamp Housing Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical |
|||
Izod Impact, Unnotched | 0.490 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical XR474F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Exterior Housing (Lamp Housing Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical |
|||
Izod Impact, Unnotched | 0.490 J/cm @Thickness 6.40 mm, Temperature -20.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature -4.00 °F |
ASTM D256 |
LG Chemical XG569C MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Unnotched | 0.490 J/cm @Thickness 3.20 mm, Temperature -20.0 °C |
0.918 ft-lb/in @Thickness 0.126 in, Temperature -4.00 °F |
ASTM D256 |
LG Chemical XG569C MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |