Polymer Property : Izod Impact, Unnotched = 0.734875 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.392266 - 1.27486 J/cm

@Temperature -30.0 - -30.0 °C
0.734875 - 2.38834 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.824 J/cm Grade Count:26
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Izod Impact, Unnotched 0.392266 - 1.27486 J/cm

@Thickness 3.20 - 6.40 mm
0.734875 - 2.38834 ft-lb/in

@Thickness 0.126 - 0.252 in
Average value: 0.824 J/cm Grade Count:26
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Izod Impact, Unnotched 0.392266 - 0.392266 J/cm

@Temperature -30.0 - -30.0 °C
0.734875 - 0.734875 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.392 J/cm Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Izod Impact, Unnotched 0.392266 - 0.392266 J/cm

@Thickness 3.20 - 6.40 mm
0.734875 - 0.734875 ft-lb/in

@Thickness 0.126 - 0.252 in
Average value: 0.392 J/cm Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..