Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.374 J/cm

@Thickness 12.7 mm
0.700 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP611 Paper Base Laminate
Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a..
Izod Impact, Unnotched 0.374 J/cm

@Thickness 12.7 mm
0.700 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP660 Paper Base Laminate
Description: Lower cost paper phenolic NEMA Grade XP. Uses natural kraft paper without pigmented cover sheet. Warm to hot punching. UL listed. Thickness Tested: 0.062", 0.125" & 0.500"
Izod Impact, Unnotched 0.374 J/cm

@Thickness 12.7 mm
0.700 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP691 Paper Base Laminate
Description: Flame resistant, room temperature punching grade. NP691 is very similar to NP612 in electrical properties and mechanical strength, with improved moisture resistance.Thickness Tested: 0...
Izod Impact, Unnotched 0.374 J/cm

@Thickness 12.7 mm
0.700 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP843 Paper Base Laminate
Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP843 has conductive surfaces only, as compared to NP842, which is conductive through..
Izod Impact, Unnotched 0.374 J/cm

@Thickness 12.7 mm
0.700 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP625 Paper Base Laminate
Description: Paper phenolic grade with better moisture resistance than NP612. Requires less heat to punch and shear than NP611.
Copyright © lookpolymers.com All Rights Reserved