Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.320 J/cm @Thickness 12.7 mm |
0.600 ft-lb/in @Thickness 0.500 in |
LW, E-48/50 |
Industrial Laminates/Norplex ES-1 Engraving Stock Description: Composed of white melamine paper core with various pigmented cover sheets.Thickness Tested: 0.0620â€, 0.125â€, and 0.500†|
|||
Izod Impact, Unnotched | 0.320 J/cm @Thickness 12.7 mm |
0.600 ft-lb/in @Thickness 0.500 in |
LW, E-48/50 |
Industrial Laminates/Norplex ES-2 Engraving Stock Description: Composed of black phenolic paper core, sub surfaces of white melamine, and various pigmented cover plies. |
|||
Izod Impact, Unnotched | 0.320 J/cm @Thickness 12.7 mm |
0.600 ft-lb/in @Thickness 0.500 in |
LW, E-48/50 |
Industrial Laminates/Norplex ES-3 Engraving Stock Description: Contains black phenolic/paper core and various colored covers impregnated with melamine resin. |
|||
Izod Impact, Unnotched | 0.320 J/cm @Thickness 12.7 mm |
0.600 ft-lb/in @Thickness 0.500 in |
CW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP611 Paper Base Laminate Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a.. |
|||
Izod Impact, Unnotched | 0.320 J/cm @Thickness 12.7 mm |
0.600 ft-lb/in @Thickness 0.500 in |
CW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP613 Paper Base Laminate Description: NP613 is constructed from electrical grade of kraft paper and a specially modified epoxy resin system. It is designed to be used in tap changers, coil support plates and terminal panels.. |
|||
Izod Impact, Unnotched | 0.320 J/cm @Thickness 12.7 mm |
0.600 ft-lb/in @Thickness 0.500 in |
CW, E-48/50 |
Industrial Laminates/Norplex NP631 Paper Base Laminate Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500" |
|||
Izod Impact, Unnotched | 0.320 J/cm @Thickness 12.7 mm |
0.600 ft-lb/in @Thickness 0.500 in |
CW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP691 Paper Base Laminate Description: Flame resistant, room temperature punching grade. NP691 is very similar to NP612 in electrical properties and mechanical strength, with improved moisture resistance.Thickness Tested: 0... |