Mechanical Properties Metric English Comments
Flexural Modulus 6.00 GPa

@Temperature 23.0 °C
870 ksi

@Temperature 73.4 °F
ISO 178
DuPont Performance Polymers Rynite® FR515 BK507 PET  (Unverified Data**)
Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr..
Flexural Modulus 6.00 GPa

@Temperature 23.0 °C
870 ksi

@Temperature 73.4 °F
50%RH; ISO 178
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL BK261 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 for injection molding. It has excellent surface appearance and gloss.Information provided by Du..
Flexural Modulus 6.00 GPa

@Temperature 23.0 °C
870 ksi

@Temperature 73.4 °F
Practical Use (Water Absorption 1.6%); ASTM-D790
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Copyright © lookpolymers.com All Rights Reserved