Polymer Property : Flexural Modulus = 6.38 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0440 GPa

@Temperature 100 °C
6.38 ksi

@Temperature 212 °F
ISO 178
DuPont Performance Polymers Hytrel® HTR8223 BK320 TPC-ET  (Unverified Data**)
Hytrel® HTR8223 BK320 is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 42D, is pigmented black with fine particle size carbon black, a..