Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.331 GPa @Temperature 90.0 °C |
48.0 ksi @Temperature 194 °F |
ASTM D790 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 0.331 GPa @Temperature 100 °C |
48.0 ksi @Temperature 212 °F |
DAM; ASTM D790 |
DuPont Performance Polymers Zytel® FE4200 BK136 Nylon 66
(Unverified Data**) Zytel® FE4200 BK136 is a low die deposit polyamide 66 extrusion resin.Information provided by DuPont Performance Polymers |