Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.30 GPa @Temperature 23.0 °C |
189 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PP HGX500707 Polypropylene, Multifiller Information provided by Polykemi AB |
|||
Flexural Modulus | 1.30 GPa @Temperature 23.0 °C |
189 ksi @Temperature 73.4 °F |
Practical Use (Water Absorption 2.4%); ASTM-D790 |
Toyobo GLAMIDE® T-656E Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 1.30 GPa @Temperature 23.0 °C |
189 ksi @Temperature 73.4 °F |
Practical Use (Water Absorption 3.0%); ASTM-D790 |
Toyobo GLAMIDE® T-808-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |