Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.00 GPa @Temperature 23.0 °C |
1310 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK261 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 for injection molding. It has excellent surface appearance and gloss.Information provided by Du.. |
|||
Flexural Modulus | 9.00 GPa @Temperature 23.0 °C |
1310 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 9.00 GPa @Temperature 23.0 °C |
1310 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 9.00 GPa @Temperature 177 °C |
1310 ksi @Temperature 351 °F |
T300 (6K); [90°]16 |
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form Fiber: T300-12K, IM7-12KInformation provided by HexCel |