Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.80 GPa @Temperature 23.0 °C |
841 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G15HSL BK083 is a 15% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 5.80 GPa @Temperature 23.0 °C |
841 ksi @Temperature 73.4 °F |
Practical Use (Water Absorption 1.9%); ASTM-D790 |
Toyobo GLAMIDE® T-402FR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 5.80 GPa @Temperature 23.0 °C |
841 ksi @Temperature 73.4 °F |
Practical Use (Water Absorption 1.75%); ASTM-D790 |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 5.80 GPa @Temperature -40.0 °C |
841 ksi @Temperature -40.0 °F |
ISO 178 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |