Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.50 GPa @Temperature 23.0 °C |
508 ksi @Temperature 73.4 °F |
Practical Use (Water Absorption 2.1%); ASTM-D790 |
Toyobo GLAMIDE® T-663G15 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 3.50 GPa @Temperature -40.0 °C |
508 ksi @Temperature -40.0 °F |
Practical Use (Water Absorption 2.4%); ASTM-D790 |
Toyobo GLAMIDE® T-714E Transparent Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 3.50 GPa @Temperature 23.0 °C |
508 ksi @Temperature 73.4 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 3.50 GPa @Temperature 80.0 °C |
508 ksi @Temperature 176 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® TY-835TC Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 3.50 GPa @Temperature -40.0 °C |
508 ksi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |