Polymer Property : Flexural Modulus = 21.4 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 21.4 GPa

@Temperature 71.1 °C
3100 ksi

@Temperature 160 °F
Dry; ASTM D790
Park Electrochemical Nelcote® P-650R Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-650R is a non-styrenated/low VOC polyester resin system that has been designed for optical clarity. P-650 exhibits good mechanical properties up to 250°F.Key Features and Benefits:Non-s..
Flexural Modulus 21.4 GPa

@Temperature 23.9 °C
3100 ksi

@Temperature 75.0 °F
Dry; ASTM D790
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 581 Quartz Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..
Flexural Modulus 21.4 GPa

@Temperature 149 °C
3100 ksi

@Temperature 300 °F
0° Direction, Dry; ASTM D790
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..