Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.10 GPa @Temperature 23.0 °C |
305 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYshine PBT D211 PBT, Modified Information provided by Polykemi AB |
|||
Flexural Modulus | 2.10 GPa @Temperature 23.0 °C |
305 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 2.10 GPa @Temperature 260 °C |
305 ksi @Temperature 500 °F |
ASTM D790 |
Saint-Gobain Meldin® 7211 CM Compression Molded Graphite and PTFE Filled Polyimide Melidin® 7211 CM is a compression molded polyimide that contains 15% graphite and 10% PTFE fillers. This grade has the lowest coefficient of friction of the Meldin® 7000 series polyimides.Spe.. |
|||
Flexural Modulus | 2.10 GPa @Temperature 80.0 °C |
305 ksi @Temperature 176 °F |
Practical Use (Water Absorption 2.1%); ASTM-D790 |
Toyobo GLAMIDE® T-663G15 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 2.10 GPa @Temperature 163 °C |
305 ksi @Temperature 325 °F |
Wet (7 day immersion at 71°C) |
Hexcel® HexPly® 954-3 Curing Cyanate Resin HexPly® 954-3 is a 350°F (177°C) curing cyanate resin with excellent resistance to moisture absorption, outgassing and microcracking. HexPly® 954-3 is formulated for autoclave or press molding u.. |
|||
Flexural Modulus | 2.10 GPa @Temperature 23.0 °C |
305 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612
(Unverified Data**) Zytel® SC315 NC010 is an unreinforced, lubricated 612 polyamide suitable for injection molding. It has been developed for applications such as parts for the healthcare industry.Information provided.. |
|||
Flexural Modulus | 2.10 GPa @Temperature 150 °C |
305 ksi @Temperature 302 °F |
ASTM D790 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |