Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 20.3 J @Temperature 23.0 °C |
15.0 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Noble Polymers Regis™ 230106 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Gardner Impact | 20.3 J @Temperature 23.0 °C |
15.0 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Noble Polymers Regis™ 235107 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Gardner Impact | 20.3 J @Temperature 23.0 °C |
15.0 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Noble Polymers Regis™ 250107 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Gardner Impact | 20.3 J @Temperature 23.0 °C |
15.0 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Noble Polymers Regis™ 275107 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Gardner Impact | 20.3 J @Temperature 23.0 °C |
15.0 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Noble Polymers Regis™ 315107 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Gardner Impact | 20.3 J @Temperature 23.0 °C |
15.0 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Noble Polymers Regis™ 190108 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |