Mechanical Properties Metric English Comments
Gardner Impact >= 434 J

@Temperature 23.0 °C
>= 320 ft-lb

@Temperature 73.4 °F
ASTM D5420
Buckeye Polymers BP FLEX D7030 BLK Thermoplastic Elastomer TPV
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..