Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 76.0 J @Temperature -30.0 °C |
56.1 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FXD121R PC Transparent/translucent PC for light diffusion special effects. MFR of 18.2. Color package may affect performance. |
|||
Dart Drop, Total Energy | 76.0 J @Temperature -30.0 °C |
56.1 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FXD121R PC (Asia Pacific) Transparent/translucent PC for light diffusion special effects. MFR of 18.2. Color package may affect performance. |