Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 60.0 J @Temperature 23.0 °C |
44.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Dart Drop, Total Energy | 60.0 J @Temperature -20.0 °C |
44.3 ft-lb @Temperature -4.00 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Dart Drop, Total Energy | 60.0 J @Temperature 23.0 °C |
44.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Dart Drop, Total Energy | 60.0 J @Temperature -20.0 °C |
44.3 ft-lb @Temperature -4.00 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Dart Drop, Total Energy | 60.0 J @Temperature 23.0 °C |
44.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Asia Pacific) Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Dart Drop, Total Energy | 60.0 J @Temperature -20.0 °C |
44.3 ft-lb @Temperature -4.00 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Asia Pacific) Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Dart Drop, Total Energy | 60.0 J @Temperature 23.0 °C |
44.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East) Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Dart Drop, Total Energy | 60.0 J @Temperature -20.0 °C |
44.3 ft-lb @Temperature -4.00 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East) Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Dart Drop, Total Energy | 60.0 J @Thickness 3.20 mm, Temperature 23.0 °C |
44.3 ft-lb @Thickness 0.126 in, Temperature 73.4 °F |
Injection Molded, Total Energy; ASTM D3763 |
Styron EMERGEâ„¢ 9500CR Polycarbonate (PC) / Polyethylene Terephthalate (PET) Overview: EMERGEâ„¢ PC/PET 9500 CR advanced resin is a polycarbonate blend with excellent chemical resistance and ignition resistance properties. This grade was designed for use in medical equipm.. |
|||
Dart Drop, Total Energy | 60.0 J @Temperature 23.0 °C |
44.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Dart Drop, Total Energy | 60.0 J @Temperature -20.0 °C |
44.3 ft-lb @Temperature -4.00 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |