Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS High flow PC+ABS. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Asia Pacific) High flow PC+ABS. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature -30.0 °C |
39.8 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Asia Pacific) PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature -30.0 °C |
39.8 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Asia Pacific) PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature -30.0 °C |
39.8 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature -30.0 °C |
39.8 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature -30.0 °C |
39.8 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® MC8002 PC+ABS AUTOMOTIVE. Low viscosity, high impact and ductility. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature -30.0 °C |
39.8 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® MC8002 PC+ABS (Asia Pacific) AUTOMOTIVE. Low viscosity, high impact and ductility. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® MC8100 PC+ABS Extrusion blowmolding grade. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® MC8100 PC+ABS (Asia Pacific) Extrusion blowmolding grade. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS High impact and ductility at 73F (23C) and -20F (-29C). |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS (Asia Pacific) High impact and ductility at 73F (23C) and -20F (-29C). |
|||
Dart Drop, Total Energy | 54.0 J @Temperature -30.0 °C |
39.8 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® FXC1200E PC+ABS (Asia Pacific) Visual Fx PC/ABS for strong fluorescent bright colors with good flow, impact and heat resistance characteristics. Consumer electronic and appliance applications uses. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® FXC1200E PC+ABS (Asia Pacific) Visual Fx PC/ABS for strong fluorescent bright colors with good flow, impact and heat resistance characteristics. Consumer electronic and appliance applications uses. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature -28.9 °C |
39.8 ft-lb @Temperature -20.0 °F |
ASTM D3763 |
Styron Pulse® 2200BG ABS + PC Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |