Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 655 MPa @Temperature 732 °C, Time 180000 sec |
95000 psi @Temperature 1350 °F, Time 50.0 hour |
|
Crucible Compaction Metals P/M Low Carbon Astroloy, Supersolvus P/M Low Carbon Astroloy is often the superalloy of choice when applications require greater ductility along with substantial strength levels. When HIP and heat treatment above the solvus temperatur.. |
|||
Rupture Strength | 655.0 MPa @Temperature 482 °C, Time 360000 sec |
95000 psi @Temperature 900 °F, Time 100 hour |
|
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
Rupture Strength | 655.0 MPa @Temperature 482 °C, Time 360000 sec |
95000 psi @Temperature 900 °F, Time 100 hour |
|
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a.. |
|||
Rupture Strength | 655.0 MPa @Temperature 482 °C, Time 360000 sec |
95000 psi @Temperature 900 °F, Time 100 hour |
|
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |