Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 34.0 MPa @Temperature 850 °C, Time 3.60e+7 sec |
4930 psi @Temperature 1560 °F, Time 10000 hour |
Stress Rupture |
AFE Technologies Cronite 657 Nickel Alloy Castings High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF.. |
|||
Rupture Strength | 34.0 MPa @Temperature 750 °C, Time 3.60e+7 sec |
4930 psi @Temperature 1380 °F, Time 10000 hour |
|
Outokumpu 4948 High Temperature Austenitic Stainless Steel Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for.. |
|||
Rupture Strength | 34.0 MPa @Temperature 850 °C, Time 3.60e+7 sec |
4930 psi @Temperature 1560 °F, Time 10000 hour |
Stress Rupture |
AFE Technologies Cronite 37Ni/18Cr/Nb No. HR32 High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF.. |