Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 127 MPa @Temperature 600 °C, Time 3.60e+7 sec |
18400 psi @Temperature 1110 °F, Time 10000 hour |
|
Outokumpu 353MA® High Temperature Austenitic Stainless Steel Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but.. |