Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 82.0 MPa @Temperature 650 °C, Time 3.60e+7 sec |
11900 psi @Temperature 1200 °F, Time 10000 hour |
|
Outokumpu 353MA® High Temperature Austenitic Stainless Steel Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but.. |
|||
Rupture Strength | 82.0 MPa @Temperature 650 °C, Time 3.60e+7 sec |
11900 psi @Temperature 1200 °F, Time 10000 hour |
|
Outokumpu 4878 High Temperature Austenitic Stainless Steel Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For .. |