Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 68.9 MPa @Temperature 871 °C, Time 360000 sec |
10000 psi @Temperature 1600 °F, Time 100 hour |
|
Special Metals INCONEL® alloy 693 INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t.. |
|||
Rupture Strength | 69.0 MPa @Temperature 871 °C, Time 3.60e+6 sec |
10000 psi @Temperature 1600 °F, Time 1000 hour |
Sheet |
Special Metals UDIMET® alloy 188 Cobalt-base Alloy UDIMET® alloy 188 (UNS R30188) is a cobalt-base alloy with excellent high-temperature strength and good oxidation resistance to 2000°F (1093°C). The high chromium level coupled with small .. |
|||
Rupture Strength | 69.0 MPa @Temperature 871 °C, Time 3.60e+6 sec |
10000 psi @Temperature 1600 °F, Time 1000 hour |
|
Special Metals UDIMET® alloy D-979 Fe-Ni Alloy UDIMET® alloy D-979 (UNS N09979) is an iron-nickel alloy designed for turbine disc applications at temperatures up to 1200-1400°F (649-760°C). Hardened by a complex precipitation of interm.. |