Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 67.0 MPa @Temperature 982 °C, Time 360000 sec |
9720 psi @Temperature 1800 °F, Time 100 hour |
2 mm sheet |
Haynes NS-163® Cobalt Alloy Alloy that brings high-temperature alloy performance at temperatures up to 2200°F (1204°C). HAYNES NS-163 alloy is a wrought cobalt-based alloy (Co–28Cr–21Fe–9Ni–1.25Tiâ€.. |
|||
Rupture Strength | 67.0 MPa @Temperature 870 °C, Time 3.60e+6 sec |
9720 psi @Temperature 1600 °F, Time 1000 hour |
|
Haynes 617 Nickel Alloy Plate Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed.. |