Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 134 MPa @Temperature 760 °C, Time 3.60e+6 sec |
19400 psi @Temperature 1400 °F, Time 1000 hour |
|
Haynes 617 Nickel Alloy Plate Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed.. |