Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 174 MPa | 25200 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Hardness, H358/30 | 174 MPa | 25200 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Hardness, H358/30 | 174 MPa | 25200 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East) VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |