Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Europe-Africa-Middle East) This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance. |
|||
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® DMX2415 PC Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Americ.. |
|||
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P.. |
|||
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe.. |
|||
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® DMX3415 PC Copolymer Lexan* DMX3415 is a co-polycarbonate resin with improved scratch resistance, high purity and optical quality.This data was supplied by SABIC-IP for the Americas region. |
|||
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance. |
|||
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health.. |
|||
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance. |
|||
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance. |
|||
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® ENH4530 PBT (Europe-Africa-Middle East) 15% GF PBT, Non-Brominated & Non-Chlorinated Flame retardant |
|||
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 430 PBT (Europe-Africa-Middle East) VALOX 430 is 33% glass reinforced, impact modified PBT injection moulding resin. |