Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 109 MPa | 15800 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® CL200 PBT+PC (Europe-Africa-Middle East) XENOY CL200 is a semi-crystalline thermoplastic blend, specially developed to obtain good low temperature impact strength combined with excellent chemical resistance to occasional solvent and gasoli.. |