Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycolac® G151 ABS (Europe-Africa-Middle East) CYCOLAC G151 is a flame retardant grade of ´new technology´ CYCOLAC which has been especially formulated to minimise many of the problems often associated with the processing of traditiona.. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Asia Pacific) Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® EXL6013 PC (Europe-Africa-Middle East) LEXAN EXL6013 is especially developed for applications requiring a high impact performance combined with an improved chemical resistance over standard polycarbonate. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® EXL6033 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with good processability.Very low temp. ductility, UV-Stabilized, UL94 V1 rated in white colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® EXL9330P PC COPOLYMER (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics Noryl V180HF PPE+HIPS (Europe-Africa-Middle East) NORYL V180HF is an unfilled, flame retardant material. It has been fully optimized w.r.t. flow and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe.. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics Noryl V190 PPE+HIPS (Europe-Africa-Middle East) NORYL V190 is an unfilled flame retardant material with a Vicat B/120 of 90°C according ISO 306. NORYL V190 is V1 at 2.0 mm according UL94 and halogen free according VDE/DIN 472 part 815.This dat.. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Asia Pacific) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Europe-Africa-Middle East) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GTX GTX954 PPE+PA (Europe-Africa-Middle East) NORYL GTX954 is an unfilled grade with improved processability and optimised heat/impact balance. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL PX1005X PPE+HIPS (Europe-Africa-Middle East) Noryl PX1005X is an unfilled, low heat resistance, halogen free (according VDE/DIN 472 part 813) flame retardant material. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL 725A PPE+HIPS (Europe-Africa-Middle East) NORYL 725A is an unfilled material, with a Vicat B/120 of 135°C according ISO 306. NORYL 725A has been designed for use in automotive interior applications, where anti-squeak is required. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL ENV105 PPE+HIPS (Europe-Africa-Middle East) NORYL ENV105 is an impact modified extrusion grade with a Vicat B/120 of 115C according ISO 306. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PA (Europe-Africa-Middle East) NORYL GTX810 is a 10% glass reinforced grade with excellent chemical resistance in combination with high stiffness and high heat resistance. |
|||
Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL PX2355 PPE+HIPS (Europe-Africa-Middle East) NORYL PX2355 is an unfilled, medium heat, low odour and low emission material with excellent heat aging performance. It has been developed for automotive interior applications, such as instrument pa.. |