Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 89.0 - 121 MPa | 12900 - 17500 psi | Average value: 104 MPa Grade Count:45 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |