Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 130 MPa | 18900 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® 2814R PC (Europe-Africa-Middle East) LEXAN 2814R is a high viscosity, 10% glass reinforced, flame retardant grade, especially developed to meet the CSTB M2 flammability rating. |
|||
Hardness, H358/30 | 130 MPa | 18900 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® ML3019 PC (Europe-Africa-Middle East) LEXAN ML3019 is a medium viscosity, 10% glass reinforced, flame retardant grade, especially designed for applications like industrial enclosures and fuse boxes requiring a low knock-out strength for.. |
|||
Hardness, H358/30 | 130 MPa | 18900 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL SE1GFN3 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN3 is a 30% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
Hardness, H358/30 | 130 MPa | 18900 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL V01550 PPE+HIPS (Europe-Africa-Middle East) NORYL V01550 is a 15 % short glass fibre reinforced, flame retardant material with a HDT/A of 130C according ISO 75. NORYL V01550 is V0 at 0.75 mm according UL94 and is halogen free according VDE/DI.. |
|||
Hardness, H358/30 | 130 MPa | 18900 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM 4001 PEI (Europe-Africa-Middle East) PTFE filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Hardness, H358/30 | 130 MPa | 18900 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East) VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles. |
|||
Hardness, H358/30 | 130 MPa | 18900 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® VX7024 PBT (Europe-Africa-Middle East) VALOX VX7024 is a 12% mineral filled PBT injection moulding resin with excellent mechanical properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Hardness, H358/30 | 130 MPa | 18900 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Hardness, H358/30 | 130 MPa | 18900 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Asia Pacific) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Hardness, H358/30 | 130 MPa | 18900 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GFN3 PPE+HIPS (Europe-Africa-Middle East) Noryl GFN3 is a standard 30 % glass filled material with a HDT/A of 145C according to ISO 75 |
|||
Hardness, H358/30 | 130 MPa | 18900 psi | ISO 2039-1 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E.. |
|||
Hardness, H358/30 | 130 MPa | 18900 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Hardness, H358/30 | 130 MPa | 18900 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GFN3V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN3V is a 30 % glass fibre reinforced material with a HDT/A of 145C according ISO 75. NORYL GFN3V has been approved for potable water applications up to 85C by the UK WFBS according BS 6920 i.. |
|||
Hardness, H358/30 | 130 MPa | 18900 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® VX4920 PBT (Europe-Africa-Middle East) VALOX VX4920 is a 20% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |
|||
Hardness, H358/30 | 130 MPa | 18900 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL PX1786G PPE+HIPS (Europe-Africa-Middle East) NORYL PX1786G is a 30 % glass filled material with a Vicat B/120 of 160 °C. |