Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00752 GPa | 1.09 ksi | 10 in/min; ASTM D412 |
PolyOne Elastamax XL 0254-15 TPU-Based Thermoplastic Elastomer
(discontinued **) This is a urethane based thermoplastic elastomer specially lubricated for auto suspension bushings. Physical Form: Pellets. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hann.. |