Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 5000 MPa
725000 psi
ISO 899-1
Lanxess Pocan® B 4215 000000 PBT, 12% Glass Fiber
PBT, 12% glass fibers, injection molding, flame retardant
Tensile Creep Modulus, 1000 hours 5000 MPa
725000 psi
ISO 899-1
Lanxess Pocan® BF 4215 000000 PBT, 12% Glass Fiber
PBT, 12% glass fibers, injection molding, flame retardant
Tensile Creep Modulus, 1000 hours 5000 MPa

@Time 3.60e+6 sec
725000 psi

@Time 1000 hour
50%RH; ISO 899-1
DuPont Performance Polymers Zytel® HTN 54G15HSLR NC010 Polyphthalamide (PPA)  (Unverified Data**)
15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR NC010 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i..