Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 2700 MPa | 392000 psi | ISO 899-1 |
Lanxess Pocan® B 7375 000000 PBT, White Pigment PBT, 25% white pigments, injection molding, improved light reflection, low tendency to warp |
|||
Tensile Creep Modulus, 1000 hours | 2700 MPa | 392000 psi | ISO 899-1 |
Lanxess Pocan® B 7425 000000 PBT, 20% Glass Spheres PBT, 20% glass spheres, injection molding, low tendency to warp, improved surface finish |
|||
Tensile Creep Modulus, 1000 hours | 2700 MPa @Strain <=0.500 % |
392000 psi @Strain <=0.500 % |
ISO 899-1 |
BASF Ultrason® E 2010 MR SW 10111 PESU Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF |
|||
Tensile Creep Modulus, 1000 hours | 2700 MPa | 392000 psi | ISO 899-1 |
BASF Ultrason® E 3010 MR UN PESU Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat.. |
|||
Tensile Creep Modulus, 1000 hours | 2700 MPa | 392000 psi | elongation <0.5%, 23°C; ISO 899-1 |
BASF Ultrason E 1010 PES Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. |
|||
Tensile Creep Modulus, 1000 hours | 2700 MPa | 392000 psi | elongation <0.5%, 23°C; ISO 899 |
BASF Ultrason E 2010 PES Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Tensile Creep Modulus, 1000 hours | 2700 MPa @Strain <=0.500 % |
392000 psi @Strain <=0.500 % |
ISO 899-1 |
BASF Ultrason® E 2010 HC PESU Information provided by BASF |
|||
Tensile Creep Modulus, 1000 hours | 2700 - 8300 MPa | 392000 - 1.20e+6 psi | Average value: 3760 MPa Grade Count:8 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |