Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 230 MPa | 33400 psi | 23°C; ISO 899; DIN 53444 |
Zell-Metall Engineering Plastics Zellamid 202 (PA 6) at 50% RH Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased... |