Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 7500 - 12000 MPa | 1.09e+6 - 1.74e+6 psi | Average value: 9170 MPa Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Tensile Creep Modulus, 1000 hours | 4500 - 12000 MPa | 653000 - 1.74e+6 psi | Average value: 7400 MPa Grade Count:10 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |